top of page

rigid Insulation
Precursor
-
Rayon Based (long/short fiber)
-
Pitch Based (short fiber)
-
Pan Based
Industrials
-
Semiconductor
-
Photovoltaics
-
High-Temp Furnaces
Manufacturing Time
-
5-30 Days
Temperature
-
Up to 3000℃
Customized
-
Design/Manufacture based on drawings
Surface Treatment
-
Graphite
-
Paper/Cloth
-
Carbon-Carbon Composites
PPM ≤ 20
Semiconductor Prodcuts
-
6/8 Inch (150mm/200mm)
-
20 Days Manufacturing Time

Sic Epitaxy

SiC/Si Crystal Growth
Photovoltaics/Furnace Prodcuts
-
Customized Size
-
8-20 Days Manufacturing Time

Tube

Customized Item

Ring

Furnaces
Raw Material

-
Grade
-
Carbonized
-
Graphitized
-
Purificated
-
-
Size(mm) up to:
-
1800×1800×200T
-
Product Specifications
Feature | Unit | Graphitized(2000℃) | Graphitized(2200℃) | Purified(2500℃) |
---|---|---|---|---|
Carbon Content | wt% | ≥99 | ≥99.9 | ≥99.99 |
Ash | ppm | ≤200 | ≤100 | ≤20 |
Bulk Density | g/cm³ | 0.13 - 0.20 | 0.13 - 0.20 | 0.13-0.20 |
Termal Conductivity(1000℃) | W/(m·K) | <0.3 | <0.3 | <0.3 |
Size | Customized | Customized | Customized | |
CTE 0℃-1000℃ | ×10⁻⁶/K | <3.5 | <3.5 | <3.5 |
CTE 0℃-2000℃ | ×10⁻⁶/K | <6.0 | <6.0 | <6.0 |
Compressive Strength | MPa | ≥0.55 | ≥0.55 | ≥0.55 |
Flexural Strength | MPa | ≥0.69 | ≥0.69 | ≥0.69 |